When casting Aluminium there are specific problems of core breakdown and removal, that are not found with ferrous castings. The lower pouring temperatures of aluminium result in lower core sand temperatures and reduced resin binder breakdown from thermal decomposition [1]. With less breakdown, the cores retain higher strength after casting and can be difficult to remove with mechanical vibration at shake-out (Figure 1). Additional time and/or effort may be needed to completely remove cores from narrow passages, increasing casting costs [2]. Thin-walled castings prone to damage during shake-out and high sand-to-metal ratios can be particularly troublesome.