The paper focuses on the mechanisms behind shrinkages in cast iron and how they can be avoided. Grey and ductile iron are unique casting alloys due to their solidification behaviour. During solidification the alloys initially contract when the temperature drops from the pouring temperature to the liquidus temperature. This contraction must always be compensated for by supply of feed metal from the gating system and often also from a feeder (riser). The paper will demonstrate that this type of feeding can only be functional until the amount of solid phase reaches a certain level. This usually happens slightly after reaching the low grey eutectic temperature. When this stage has been reached a balanced precipitation rate and amount of graphite will make it possible to compensate for contraction of remaining liquid and the eutectic austenite. The proper balance is crucial as the precipitation of graphite is associated with a volume expansion, which if too high will cause mould wall movement and increase shrinkage tendency. Too low precipitation will lead to micro-shrinkages. The paper describes how optimization of the gating system in many cases makes it possible to eliminate feeders for supply of the initial feed metal. After the low eutectic temperature is reached the contraction can be eliminated by careful control of graphite precipitation using a combination of chemical and adaptive thermal analysis. Through proper control of the feeding sequences it is possible to produce certain ductile iron castings in green sand moulds without feeders!
Full paper (PDF)
PDF · 184.93 KB · Document in English
The full paper is available to members of the institute only.
Log in to downloadDetails
AuthorsRudolf Val. Sillén
Organisation* NovaCast Technologies AB, Sweden
Event67th World Foundry Congress
TopicEngineering
Document languageEnglish
Year2006