Numerical simulations of solute redistribution and microstructure evolution during solidification, post-solidification cooling, and solution heat treatment have been extended to multi-phase, multi-component Al-Si-Cu-Mg alloys. The basic models that have been applied to binary and ternary systems have been modified to handle the extra degrees of freedom in quaternary and higher order systems, which are more representative of commercial casting alloys.
During solidification Si and Mg diffusion is extensive and microsegregation of Si and Mg in the dendrite cores at the end of solidification is negligible. Diffusion of Cu through the dendrite cores controls the extent of microsegregation of Cu in the as-solidified alloy. The presence of small amounts of Mg enhances diffusion of Cu, and the diffusivity of Cu in multiphase interdendritic regions is several multiples of the diffusivity through the single-phase dendrite cores.
Substantial solute redistribution occurs during post-solidification cooling in sand or permanent molds. Si, in particular, diffuses from dendrite cores to the interdendritic regions as the solubility of Si in the interdendritic α-Al phase decreases sharply with decreasing temperature.
During solution heat treatment the redistribution of solute that occurs during post-solidification cooling is reversed quickly. The nonequilibrium amounts of θ-phase and Q-phase that are distributed in the interdendritic regions between secondary dendrite arms at the end of solidification are reduced to their equilibrium amounts within a few hours. Nonequilibrium phases distributed in the grain boundaries and between primary dendrite branches require ten or more hours to reduce to their equilibrium amounts.