To produce partially composed metal matrix composites, a new spontaneous infiltration process was developed. The infiltration process should be controlled by a wetting phenomenon; therefore, we discussed how to improve the wettability based on the reactive wetting concept. The SiC preforms infiltrated at 1173 K without pressure in air using Al-Si-3Mg melts. The 60mmφ × 30mmh preforms were fabricated using a water glass binder with Fe2O3 powder and for 2h and dried at 393K for 12h before the infiltration. The infiltration rate was measured using a load sensor based on the weight change of the preform with the infiltration. It was confirmed that the infiltration rate was accelerated by the Fe2O3 powder addition.
Full paper (PDF)
PDF · 394.08 KB · Document in English
The full paper is available to members of the institute only.
Log in to downloadDetails
AuthorsHideo Nakae, Yuuji Araoka and Yuuta Sugiyama
Organisation* Waseda Univ. Japan; **Graduate Students, Waseda Univ.,Japan
Event67th World Foundry Congress
Document languageEnglish
Year2006