Hot tearing in certain cast metals continues to bother metal casters. A number of casting parameters affect the susceptibility to hot tearing. Experiments were conducted on Al-1%Sn alloys. Al-1%Sn is a high freezing range alloy known to be extremely prone to hot tear cracking. Effects of grain refinement and presence of iron and nickel have been investigated by making use of a ring type casting with a steel core. Al-5Ti- 1B was used as the grain refiner. Optical and scanning electron microscopy was used in the study. The results showed that contrary to some published work, grain refinement alone could not eliminate hot tearing. Average hot tear length decreased with increased grain refinement and the minimum being achieved was at 5% by weight of Al- 5Ti-1B addition. Both iron and nickel have positive effects in minimizing hot tear formation. SEM studies have shown that with iron there is an Al- Sn-Fe rich phase in the form of a leaf like structure believed to be providing anchorage to the adjacent grains and thus overcoming hot tear.
Full paper (PDF)
PDF · 248.58 KB · Document in English
The full paper is available to members of the institute only.
Log in to downloadDetails
AuthorsG. L. Datta and D. Benny Karunakar
OrganisationMechanical Engg. Dept., IIT, Kharagpur, India
Event67th World Foundry Congress
TopicLight alloys
Document languageEnglish
Year2006